Improving the strength and softness of crust leather through pressure treatment
Introduction
Retanning and fatliquoring have a major impact on the characteristics of leather, whereas dyeing and the finishing concentrate on the appearance of the leather. Various retanning agents and fatliquoring agents have been developed to improve the softness and mechanical strength of leather, parameters that are important to the buyers of leather. However, although chemicals can be added to a process to improve the leather quality, doing so increases production costs, as well as contributing to effluent production.
The addition of chemicals to leather can significantly change the structural parameters of leather, such as the porosity, dispersion of fibres and fibre diameter. These in turn impact on the tensile and tear strength of the leather, which are important characteristics of leather.
The performance of leather is greatly affected by its pore structure, and compression is an important method to improve the pore structure of the material and increase performance, but this method is rarely used in the leather industry. Hot pressing is widely used in many other industries to improve the porosity, structure and strength of the materials being manufactured.
This research was carried out to investigate crust leather properties under different pressures and to analyse its microstructure.
Experimental
Leather samples were subjected to a 1-hour treatment at pressures of 0 MPa, 7.5 MPa, 15 MPa, 22.5 MPa, 30 MPa, and 37.5 MPa using a single-layer hot press at 25°C. After 48 hours of standard air conditioning at 20°C and 65% humidity, the mechanical properties of the samples were tested.
Tensile strength, tear strength, elongation at break and softness were determined using standard methods.
The morphology of the crust leather fibre structure was determined through a scanning electron microscope at magnifications of 100× and 500×. The pore structure of samples was ascertained using a mercury intrusion porosimeter and automatic physical adsorption instrument.
Results
The thickness of crust leather samples subjected to varying pressures are shown in Table I. Sample thicknesses were reduced with increasing pressure. The thickness changed rapidly at the beginning from 2.03 to 1.72 mm under 7.5 MPa, while the thickness remained 1.58 mm under 15-22.5 MPa. The pressure was further increased to 30-37.5 MPa, and as a result, the thickness was also reduced to 1.36 mm.

Table 1. Crust leather thickness as a result of the applied pressure. (Image source: JALCA 120, 107 – 114 (2025)
The longitudinal and transverse tensile strength are displayed in Figure 1a. The longitudinal and transverse tensile strengths typically displayed an increasing trend as pressure increased. Longitudinal tensile strength increased by 108%, from 32.6 to 67.9 MPa, while transverse tensile strength increased from 23.8 to 47.8 MPa. This could be due to the increase in fibre density under high pressure. Figure 1b displays the longitudinal and transverse tear strength of crust leather. In contrast to the tensile strength, the tear strength first reduced, then improved, and then decreased. It reached its maximum value (L: 310 N/mm; T: 367 N/mm) at 30 MPa external pressure, while the tear strength reduced at 37.5 MPa, which could be associated with the early tear curves’ inflection point (Figure 1e, f). Furthermore, the elongation at break (Figure 1c) first reduced, then increased, and resembled the untreated sample following treatment with 22.5 MPa. The elongation at break and tear strength displayed the opposite tendency, while the tensile strength in the L direction was higher than that in the T direction.
The lower pressure treatment resulted in a reduction in the softness of the crust leather to only 3.2 mm, whereas the softness of the crust leather treated with 30 MPa was comparable to the untreated sample (>5mm), as shown in Figure 1d. This demonstrates that the mechanical properties of crust leather can be improved by proper pressure without reducing its softness.

(Image source: JALCA 120, 107 – 114 (2025)
Conclusion
In this study, the crust leather was treated with different pressures, and the mechanical properties of the treated samples were investigated, including tensile strength, tear strength, elongation at break, and softness. With the increase of pressure, the tensile strength of crust leather progressively enhanced, while the elongation at break, tear strength, and softness all decreased first and then increased. The structural evaluation of the samples (data not shown in this summary due to article length limitations) showed that, without the use of chemicals, external pressure changed the fiber structure, causing the fibers to be closely packed and affecting D-spacing and fibril diameter. The tensile strength of the crust leather was enhanced by the small pores formed in the leather, which also improved the fiber density. With the change of pressure, the crust leather showed a significant variation in mechanics and structure.
External pressure on the crust leather improved the fibre structure without the use of chemicals or a reduction in softness, resulting in closely packed fibres that increased tensile strength, decreased average pore diameter, and enhanced specific surface area and fibre density.
This research shows that it may be possible to improve the strength and softness properties of crust leather simply by treating the crust leather with a pressure plate for 1 hour at a temperature of 25ºC and may well be a clean method for producing high-performance crust leather or leather products.
This article is a summary of the paper “Effect of Pressure Treatment on Structure and Mechanics of Crust Leather”. Journal of the American Leather Chemists Association (JALCA) Vol 120, 107 - 114 (2025).
Footwear Industry Articles
- Manufacturer-buyer event: Among the retailer commentsKim Cunniffe, Kingsmead ShoesOur buyers found some suppliers they were unaware of, and a few possibilities in terms of product. We haven’t yet taken this forward, but we will do so.Hassen Ismail, Fashion WorldIt was more-or-less what you expect of local manufacturing in terms of styling, quality, and price.We have asked for samples. ...moreManufacturer-buyer event: Among the manufacturer commentsThe 2-day Retail Buyer Engagement & Manufacturer Onboarding Programme on 01 and 02 July was part of an effort to kickstart the R-CTFL Masterplan – which, from a footwear perspective at least, has appeared stalled.It was sponsored by the International Labour Organisation (ILO) and implemented through the R-CTFL Masterplan Footwea ...moreSAFLEC AGM 2026: A year marked by resilienceOn behalf of the Board of Directors, it is my pleasure to welcome all our members and stakeholders to the 24th Annual General Meeting of the South African Leather & Footwear Export Council (SAFLEC).The Annual General Meeting provides us with an opportunity not only to reflect on the performance of the Council over the past financial y ...more
Leather Industry Articles
- Beyond the data trap: Why better decisions matter more than just more dataOn 1st July 2026 I presented at the FILK Leather Days conference and asked the delegates to consider “Sustainability through a new lens: resetting how we view impacts in the leather value chain”. This month’s article therefore explores this idea a little more with a focus on how we view data and whether it can blind us t ...moreOrganic cotton at the crossroads: Ideology, evidence, and the road aheadWashington, DC, U.S.A. (23 June 2026) — Organic cotton occupies one of the most contentious spaces in global agriculture. While praised by brands and consumers for its environmental ideals, it also faces persistent questions about yield stability, certification integrity, and scalability. The current edition of The ICAC Recorde ...moreFifteen million sheep in the UK to share among shearersAccording to the UK government, its sheep population decreased over the past year by 1.7% but that still leaves a flock of over 30 million. For comparison, the domestic flock in South Africa numbers about 21 million and New Zealand has some 23 million. Australia, with more than 70 million, has a wool clip of approximately 325,000 tonnes. ...more
PPE Industry Articles
- Statistical shape modelling for population-specific respirator design: Addressing fit failure in South African populationsRespirators are widely regarded as the last line of defence against hazardous airborne exposures. Whether protecting healthcare workers from tuberculosis, laboratory personnel from infectious samples, or workers exposed to carcinogenic dusts and fumes, respirators are often relied upon when other controls cannot eliminate exposure. This r ...moreSAPEMA demands action against retailer Curve Gear over selling noncompliant safety footwearThe Southern African Protective Equipment Marketing Association (SAPEMA) has reported retailer Curve Gear to the National Regulator for Compulsory Standards (NRCS) for selling “possibly noncompliant” safety footwear.The allegation is because Curve Gear’s safety footwear doesn’t carry mandatory marking: Its NRCS app ...morePremier Workwear: Engineered protection for Africa’s industrial workforceIn high-risk industrial environments, protective clothing is far more than a uniform requirement — it is a critical component of workplace safety, operational reliability and regulatory compliance. For procurement professionals, safety managers and operational leaders, selecting the right supplier means finding a partner capable of ...more